Title Characteristics and kinetics study of spherical cellulose nanocrystal extracted from cotton cloth waste by acid hydrolysis
ID_Doc 14738
Authors Doan, TKQ; Chiang, KY
Title Characteristics and kinetics study of spherical cellulose nanocrystal extracted from cotton cloth waste by acid hydrolysis
Year 2022
Published Sustainable Environment Research, 32, 1
Abstract This work investigated the extraction of spherical cellulose nanocrystal (spherical CNC) from cotton cloth waste (CCW) using sulfuric acid without ultrasound treatment during the hydrolysis process, producing a yield of 31%. The cellulose was first extracted through alkali, decoloring, and hydrochloric acid treatment. Then the cellulose was hydrolyzed using 55 wt% sulfuric acid with various acid to cellulose ratios, including 30:1, 40:1, and 50:1 mL g(- 1). The resulting CNC was characterized by morphological structure, functional groups, crystalline structure, elemental compositions, thermal degradation kinetic, and zeta potential. The analytical results revealed that the acid to cellulose ratios significantly influenced the properties of CNC obtained. The morphological structure showed that when the acid to cellulose ratio was 30:1 and 40:1 mL g(- 1), the rod-like CNC was observed with a length of 53 +/- 19 nm and 49 +/- 13 nm; a width of 6.6 +/- 1.3 nm and 4.3 +/- 2.0 nm, respectively. However, when the acid to cellulose ratio was further increased to 50:1 mL g(- 1), the nanocellulose morphology turned to be spherical, with an average diameter of 14.4 nm. Furthermore, spherical CNC exhibited better characteristics consisting of crystallinity index (94.6%) and stable dispersibility with zeta potential value - 46.8 mV than rod-like CNC. However, the thermal stability of spherical CNC was slightly lower than that of rod-like CNC. The kinetic results indicated that the activation energy of spherical CNC ranged from 134 to 423 kJ mol(- 1), which is lower than that (145 to 651 kJ mol(- 1)) of rod-like CNC ranging from. This study showed that the CCW is a potential low-cost cellulose source to manufacture spherical CNC and a good example for developing a circular economy.
PDF

Similar Articles

ID Score Article
13840 Espíndola, SP; Pronk, M; Zlopasa, J; Picken, SJ; van Loosdrecht, MCM Nanocellulose recovery from domestic wastewater(2021)
20565 Chia, MR; Phang, SW; Razali, NSM; Ahmad, I Approach towards sustainable circular economy: waste biorefinery for the production of cellulose nanocrystals(2024)Cellulose, 31, 6
9259 Sathasivam, T; Sugiarto, S; Yew, MPY; Oh, XY; Chan, SY; Chan, BQY; Tim, MJ; Kai, D Transforming textile waste into nanocellulose for a circular future(2024)Nanoscale, 16.0, 30
13131 Yu, YH; Guo, W; Qu, JJ; Wang, S; Wang, XG; He, Y; Yang, Y; He, Q; Liu, XD Preparation and characterization of dialdehyde cellulose nanocrystals from the waste nutshell(2023)
8092 Basak, M; Gandy, E; Lucia, LA; Pal, L Polymer upcycling of municipal solid cellulosic waste by tandem mechanical pretreatment and maleic acid hydrolysis(2023)Cell Reports Physical Science, 4, 12
8393 Kasapoglu, ED; Kahraman, S; Tornuk, F Extraction Optimization and Characterization of Cellulose Nanocrystals from Apricot Pomace(2023)Foods, 12.0, 4
9711 Gupta, V; Ramakanth, D; Verma, C; Maji, PK; Gaikwad, KK Isolation and characterization of cellulose nanocrystals from amla (Phyllanthus emblica) pomace(2023)Biomass Conversion And Biorefinery, 13.0, 17
18585 Rebec, KM; Turk, J; Kunaver, M Quantifying the environmental implication of cotton-Fiber-based Nanocrystalline cellulose: A life-cycle assessment(2024)
10605 Babicka, M; Wozniak, M; Bartkowiak, M; Peplinska, B; Waliszewska, H; Zborowska, M; Borysiak, S; Ratajczak, I Miscanthus and Sorghum as sustainable biomass sources for nanocellulose production(2022)
8534 Costa, C; Viana, A; Silva, C; Marques, EF; Azoia, NG Recycling of textile wastes, by acid hydrolysis, into new cellulosic raw materials(2022)