Title Improving the Performance of Mortars Made from Recycled Aggregates by the Addition of Zeolitised Cineritic Tuff
ID_Doc 15564
Authors Martín, DA; Costafreda, JL; Costafreda, JJL; Presa, L
Title Improving the Performance of Mortars Made from Recycled Aggregates by the Addition of Zeolitised Cineritic Tuff
Year 2022
Published Crystals, 12, 1
Abstract Metropolitan construction and demolition waste (CDW) is currently an important source of recycled materials that, despite having completed their useful life cycle, can be reincorporated into the circular economy process (CEP); however, the recycling process is very selective, and waste material is not always fully satisfactory due to the intrinsic nature of the waste. This work aims to demonstrate and establish how to increase the effectiveness of the construction and demolition waste in more resistant mortars, by mixing it with zeolitised cinerite tuff (ZCT) at varying normalised proportions. To attain the objectives of this research, a series of tests were done: First, a chemical, physical and mineralogical characterisation of the CDW and the ZCT through XRF, XRD, SEM and granulometric methods. Second, a technological test was made to determine the mechanical strength at 7, 28 and 90 days of specimens made with Portland cement (PC) and mixtures of PC/CDW, PC/ZCT, and PC/CDW-ZCT. The results obtained through the characterisation methods showed that the sample of construction and demolition waste consisted of the main phase made of portlandite and tobermorite, and by a secondary phase consisting of quartz, ettringite and calcite; whereas the ZCT has a main phase of mordenite and a secondary phase of smectite (montmorillonite), amorphous materials consisting of devitrified volcanic glass, quartz and plagioclase. Mechanical strength tests established that specimens made with PC/CDW mixtures have very discreet compressive strength values up to 44 MPa at 90 days, whereas specimens made with PC/ZCT mixtures achieved a remarkably high mechanical strength consisting of 68.5 MPa. However, the most interesting conclusion in this research is the good result obtained in mechanical strength of the specimens made up of mixtures of PC/CDW-ZCT, which increased from 52.5 to 62 MPa at 90 days of curing; this fact establishes the positive influence of ZCT on waste in the mortar mixtures, which permits the authors to establish that the objective of the work has been fulfilled. Finally, it can be argued that the results obtained in this research could contribute to more effective use of construction and demolition waste in metropolitan areas.
PDF https://www.mdpi.com/2073-4352/12/1/77/pdf?version=1641479316

Similar Articles

ID Score Article
10920 Rosado, S; Costafreda, J; Martín, D; Presa, L; Gullón, L Recycled Aggregates from Ceramic and Concrete in Mortar Mixes: A Study of Their Mechanical Properties(2022)Materials, 15, 24
6564 Borges, PM; Schiavon, JZ; da Silva, SR; Rigo, E; Neves, A; Possan, E; Andrade, JJD Mortars with recycled aggregate of construction and demolition waste: Mechanical properties and carbon uptake(2023)
9188 Jesus, S; Pederneiras, CM; Farinha, CB; de Brito, J; Veiga, R Reduction of the Cement Content by Incorporation of Fine Recycled Aggregates from Construction and Demolition Waste in Rendering Mortars(2021)Infrastructures, 6.0, 1
21822 Ulas, MA; Culcu, MB; Ulucan, M Valorization of recycled aggregates to eco-efficient lightweight self-compacting mortars: Studies on microstructure, mechanical, durability, environmental, and economic properties(2024)
14086 Sargent, P; Sandanayake, M; Law, DW; Hughes, DJ; Shifa, F; Borthwick, B; Scott, P Strength, mineralogical, microstructural and CO2 emission assessment of waste mortars comprising excavated soil, scallop shells and blast furnace slag(2024)
18473 Gutiérrez, ER; Ferrández, D; Atanes-Sánchez, E; de Pablo, MR Physico-Mechanical Characterization of Masonry Mortars for Sustainable Construction: Experimental Study with Four Different Aggregates(2024)Sustainability, 16.0, 14
13850 Volpintesta, F; Finocchiaro, C; Barone, G; Mazzoleni, P; Paris, E Compositional Differences in Construction and Demolition Wastes (CDWs) for Geopolymer Mortars: A Comparative Study Using Different Precursors and Alkaline Reagents(2024)Minerals, 14, 4
6276 Juan-Valdés, A; Rodríguez-Robles, D; García-González, J; Gómez, MISD; Guerra-Romero, MI; De Belie, N; Morán-del Pozo, JM Mechanical and microstructural properties of recycled concretes mixed with ceramic recycled cement and secondary recycled aggregates. A viable option for future concrete(2021)
5108 Vachuska, V; Vachuska, J; Volosinová, D; Vachuska, A Effective Use Of Construction And Demolition Waste And Stone Dust In Construction For The Production Of Manufactured Aggregates In Two Pilot Regions Of The Czech Republic(2022)Environment Protection Engineering, 48.0, 2
12848 Belkadi, AA; Kessal, O; Chiker, T; Achour, Y; Rouabhi, A; Messaoudi, O; Khouadjia, MLK Full Factorial Design of Mechanical and Physical Properties of Eco-mortars Containing Waste Marble Powder(2023)Arabian Journal For Science And Engineering, 48.0, 4
Scroll