Knowledge Agora



Scientific Article details

Title Incorporation of the Multi-Layer Plastic Packaging in the Asphalt Binders: Physical, Thermal, Rheological, and Storage Properties Evaluation
ID_Doc 22207
Authors Qabur, A; Baaj, H; El-Hakim, M
Title Incorporation of the Multi-Layer Plastic Packaging in the Asphalt Binders: Physical, Thermal, Rheological, and Storage Properties Evaluation
Year 2022
Published Polymers, 14.0, 24
DOI 10.3390/polym14245396
Abstract The amount of residual Multi-layer Plastic Packaging (MPP) in Canada has greatly increased in the last two decades, which has economic and environmental consequences. MPP is primarily made up of two or more layers of Polyethylene (PE), Polyester (PET), Nylon (NY), and Metalized Polyester (METPET). While MPP has not been used as an asphalt modifier, some of the materials commonly found in MPP, such as PE and PET, have also been successfully used as asphalt modifiers. Nevertheless, a few recent studies have demonstrated the potential for reusing MPP as an asphalt modifier to improve asphalt pavement performance. Recycling post-industrial MPP instead of using raw polymers could lead to economic and environmental benefits. However, a comprehensive study to evaluate MPP as a viable asphalt additive is lacking. The main objective of this study is to evaluate the feasibility of using MPP as an asphalt modifier via the wet method, considering the physical, thermal, rheological, and storage properties of the MPP-modified binder at different MPP concentrations (2%, 4%, and 8%) in asphalt cement (PG 58-28). MPP-modified binders were evaluated using the following instruments: Differential Scanning Calorimeter (DSC), Thermogravimetric Analysis (TGA), Superpave Dynamic Shear Rheometer (DSR), Rotational Viscosity (RV), and Environmental Scanning Electron Microscopy (ESEM). Test results indicated that the incorporation of MPP has a strong potential to improve permanent deformation resistance at high temperatures. In addition, MPP shows a moderate impact on fatigue cracking performance at intermediate temperatures. Overall, in low-temperature climates, using less than 4% of MPP additives would offer higher fatigue damage resistance along with adequate permanent deformation. In high-temperature climates, higher concentrations of additives may be preferable to resist permanent deformation. Finally, MPP is a challenge for existing recycling systems, and its incorporation into asphalt applications may develop more sustainable materials that would contribute to circular economy principles.
Author Keywords multi-layer plastic packaging (MPP); recycling; asphalt cement; fatigue; permanent deformation; circular economy
Index Keywords Index Keywords
Document Type Other
Open Access Open Access
Source Science Citation Index Expanded (SCI-EXPANDED)
EID WOS:000904254400001
WoS Category Polymer Science
Research Area Polymer Science
PDF https://www.mdpi.com/2073-4360/14/24/5396/pdf?version=1670584653